Ürün Adı: 4 Core MM 50,125 Çelik Zırh Dış Mek OM2 Fiber Optik
Ürün Bilgisi
| ÖZELLİKLER | BİRİM | DEĞERLER | TEST STANDARTLARI | 
| TENSILE STRENGTH AT BREAK | kN | >1.2 | EN 60794.1.E1 | 
| BREAKING TENSILE STRENGTH | kN | >1.5 | EN 60794.1.E1 | 
| CRUSH RESISTANCE | N/cm | >200 | EN 60794.1.E3 | 
| REPEADING BENDING RADIUS | mm | <20xD | EN 60794.1.E6 | 
| SINGLE BENDING RADIUS | mm | <15xD | EN 60794.1.E6 | 
| TORSION | +90° C,8 | possitive | EN 187 000 M 508 | 
| IMPCAT | kN | >1 | EN 187000 M 504 | 
| TEMPERATURE | 
 | 
 | EN 60794.1.E11 | 
| OUTER SHEATH | 
 | 
 | 
 | 
| DENSITY | g/cm³ | >20 | ASTM D 638 | 
| TENSILE STRENGTH AT BREAK | N/mm² | >400 | ASTM D 638 | 
| ELONGATION AT BREAK | % | 2/10 | ASTM D 1693 | 
| E.S.C.R. (%10 lgepal C-630) | >500 hours | 2/10 | ASTM D 746 | 
| BREAKING COLD | <-75°C | 2.5+0.5 | ASTM D 1603 | 
| CARBON BLACK RATE | % | <0.950 | ASTM D 792 METOT A | 
| OXIGEN INDUCTION TIME | 200°C | >25 | IEC 811.4.2 B | 
| TUBE GEL | 
 | 
 | 
 | 
| DENSITY (25°C) | g/cm³ | +0.05 | DIN 51 757 | 
| DROP POINT (24 HOUR) | °C | aooropriate | IEC 811.5.1 B | 
| DRIP POINT (24 HOUR) | °C | >70 | REA PE 39 | 
| FLASH POINT | °C | >230 | ISO 2592 | 
| OIL SEPERATION (150°C, 24 HOUR | % | 0 | FTM STD 791 C | 
| VOLATILITY | % | <2 | FTM STD 791 C | 
| WATER ARMOUNT | % | <0.05 | DIN 51 777 | 
| ACID VALUE (100°C) | % (mg KOH/g) | <0.01 | DIN 53 402 | 
| ABRATION | 
 | posıtıve | IEC 811.5.1 | 
| PENETRATION (25°C / -30°C) | 1/10 mm | >150 | ISO 2137 | 
| OXIGEN INDUCTION TIME (180°C) | minute | >20 | IEC 811.4.2 B | 
| 100-500V (100°) | Ω x m | >10 | ASTM D 1169 | 
| 100-500V (23°) | Ω x m | 
 | ASTM D 1169 | 
| LOSE TUBE | 
 | >10,11 | 
 | 
| DENSITY | g/cm³ | 1.31+0.03 | ISO 1183 | 
| WATER ABSORPTION (23°C) | % | <0.45 | DIN 53 495 | 
| TENSILE STRENGTH AT BREAK | N/mm² | <30 | ISO 527 | 
| ELONGATION AT BREAK | % | >50 | ISO 527 | 
| E-MODULUS | N/mm² | >2200 | ISO 527 | 
| SHORE | Shore D | >78 | DIN 53 505 | 
| MELTING TEMPERATURE (DSC) | °C | >220 | ISO 3146 C | 
| LIN. THERMAL EXT. COEFF. (-23<<+80°C) | °K-1 x10-4 | <1.3 | 
 | 
| E-GLASS YARN | 
 | 
 | 
 | 
| DENSITY | g/cm³ | offered | offered | 
| TENSILE STRENGTH AT BREAK | 
 | 